- C92700 Alloy

Thermal Conductivity Btu/ sq ft/ ft hr/ °F at 68°F. 27.2. Coefficient of Thermal Expansion 68-392 10 to -6 power per °F (68 – 392°F) 10. Specific Heat Capacity Btu/ lb /°F at 68°F.

contact
Density lb/cu in. at 68°F: 0.317

Leaded Tin Bronze – Copper Casting Alloy UNS C92700